Customization: | Available |
---|---|
After-sales Service: | Available |
Warranty: | Lifetime Warrancy |
Still deciding? Get samples of US$ 1999/Piece
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Barrel Diameter: | φ300-φ1050 mm | Casting Type: | Centrifugal Casting |
Material: | Enhanced High-Speed Steel (HSS) | Hardness (For Reference) |
82-88HSD |
Material Code: | H3-B | Hardness Drop | ≤3HSD |
Material Instruction: | It's a newly developed wear-resistant material tailored by our company to meet the diverse process conditions of hot-rolled strip production lines. | Rolling Temperature | 780ºC-1100ºC |
Use Periods | 8-10 Cycles | Dressing | 1.0-1.5mm |
Application | work rolls in four-high roughing and finishing mills for hot-rolled strip steel (including endless rolling). |
1. Superior Wear Resistance and High-Temperature Hardness
• Excellent resistance to wear and thermal softening under high-temperature conditions.
• Strong resistance to thermal cracking, roll marks, and surface defects, with uniform wear ensuring consistent roll profile.
2. Stable Roll Shape and Plate Shape Control
• Advanced heat treatment ensures uniform material properties with fine grain structure.
• Roll body hardness uniformity ≤3HSD, and working layer hardness variation ≤3HSD.
3. High Mechanical Strength and ToughnessPrevents oxidation layer peeling and working layer spalling during operation
• High tensile strength (≥800MPa) with excellent impact toughness and thermal cracking resistance.
• Prevents oxidation layer peeling and working layer spalling during operation.
4. Outstanding Fatigue Resistance
• Exceptional wear resistance and fatigue performance reduce single-time grinding volume.
• Each regrinding provides an operational cycle exceeding 12 hours, with a total rolling capacity over three times that of high chromium cast iron rolls.
Chemical Composition
Material | HBW Patented Chemical Composition (%) | |||||||||||
C | Si | Mn | Cr | Ni | Mo | V | W | P & S | Nb | Co | Others | |
HBW's HSS | 1.5 - 2.10 |
0.20 - 1.0 |
0.30 - 1.0 |
3.00 - 6.00 |
0.50 - 1.50 |
3.0 - 7.0 |
2.0 - 8.0 |
1.0 - 8.0 |
≤0.03 | Depends on HSS Grade | ||
Properties | Barrel | Core | |
Tensile Strength | ≥700MPa | ≥450MPa | |
Compressive Strength | ≥2500MPa | -- |
Metallographic Structure